<bibimport/>
Author: Hans-Jürgen Schwarz
Back to Decay Pattern
Abstract
Für Baukeramik typische Schadensbilder werden vorgestellt und anhand von Abbildungen erläutert.
Decay Pattren on Architectural Ceramics
Ziegelschäden
Salt-induced damage to bricks are common.
Damage to bricks can look like this:
Scaling(?)
- Decay pattern on a brick of the St.Jakobi church in Perleberg
Figure 1: The damaged brick shows a scaly surface, which was caused by crystallizing salts.
Figure 2: Photo of a thin section in polarized light. The grey parallel crystals are gypsum.
Figure 3: Photomicrograph as Fig 2 but with crossed polarisers. It is clearly seen that the plaster is both responsible for the damage and on the other hand, he acts in this case as a kind of glue that holds together the broken brick pieces. With the removal of the original plaster the brick material would be lost.
Back Weathering
- Schäden an einem Gebäude in Lüneburg
Figure 4: Salze schädigen einen Formstein
Figure 5: Salzschäden wirken unter Oberfläche einer Beschichtung.
Efflorescences
- Efflorescences on Architectural Ceramics
Abbildung 6: Salzrasen auf einer Fußbodenplatte
Abbildung 7: Salzkruste aus Karbonat-Salzen an einem Pfeiler aus Formsteinen. Ursache waren in diesem Fall Verpressungen mit Zementsuspension
Abbildung 8: Ausktistallisierende Salze verdeutlichen das Craqueleé deines glasierten Ziegels. Mit der Zeit werden die Salze zu Schäden an der Glasur führen.