Architectural Ceramics: Difference between revisions
Jump to navigation
Jump to search
Line 17: | Line 17: | ||
'''Deterioration of brickwork''' | '''Deterioration of brickwork''' | ||
Salt-induced damage to bricks is common. | Salt-induced damage to bricks is very common. | ||
'''Glazed architectural ceramics''' | '''Glazed architectural ceramics''' | ||
The glaze on building ceramics prevents the transport of moisture and salts. Often however, the glaze shows "crazing" (a fine network of fissures or cracks) allowing moisture transport through it. And therefore, if salts are present, they will crystallize around these fissures as well as below the glazing around them, leading to | The glaze on building ceramics prevents the transport of moisture and salts. Often however, the glaze shows "crazing" (a fine network of fissures or cracks) allowing moisture transport through it. And therefore, if salts are present, they will crystallize around these fissures as well as below the glazing around them, leading to its spalling. | ||
Revision as of 13:52, 26 January 2013
Author: Hans-Jürgen Schwarz
English Translation by Sandra Leithäuser
Back to Decay Pattern
Abstract[edit]
Typical deterioration patterns for architectural ceramics are discussed and explained.
Decay patterns of architectural ceramics[edit]
Deterioration of brickwork
Salt-induced damage to bricks is very common.
Glazed architectural ceramics
The glaze on building ceramics prevents the transport of moisture and salts. Often however, the glaze shows "crazing" (a fine network of fissures or cracks) allowing moisture transport through it. And therefore, if salts are present, they will crystallize around these fissures as well as below the glazing around them, leading to its spalling.