Typical damage patterns are presented and explained.
Decay Pattern of Architectural Ceramics
Ziegelschäden
Salt-induced damage to bricks are common.
Damage to bricks can look like this:
Glazed Architectural Ceramics
The glaze of a glazed building ceramics prevents both the transport of moisture and salts. Often however glaze is crackled, which allows a capillary moisture transport. The Craquelée particularly clear shows an existing salt load, which consequently often leads to the spalling of the glazes.
Some examples of salt-contaminated glazed building ceramics are shown here.
Scaling(?)
- Decay pattern on a brick of the St.Jakobi church in Perleberg
Figure 3: Photomicrograph as Fig 2 but with crossed polarisers. It is clearly seen that the plaster is both responsible for the damage and on the other hand, he acts in this case as a kind of glue that holds together the broken brick pieces. With the removal of the original plaster the brick material would be lost.
Back Weathering
- Schäden an einem Gebäude in Lüneburg
Efflorescences